Chemical properties
Property | Value |
---|---|
Aluminio | 8 - 10 % Show Material materials with Aluminio of 8 - 10 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Manganeso | 1.5 - 2.5 % Show Material materials with Manganeso of 1.5 - 2.5 % |
Otro | Rest Cu, total 1.5 |
Plomo | 0.03 % Show Material materials with Plomo of 0.03 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Zinc | 1 % Show Material materials with Zinc of 1 % |