Chemical properties
Property | Value |
---|---|
Aluminio | 0.15 % Show Material materials with Aluminio of 0.15 % |
Berilio | 1.85 - 2.1 % Show Material materials with Berilio of 1.85 - 2.1 % |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % |
Níquel | 0.2 - 0.4 % Show Material materials with Níquel of 0.2 - 0.4 % |
Otro | Rest Cu, total 0.5 |
Plomo | 5E-3 % Show Material materials with Plomo of 5E-3 % |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % |
Titanio | 0.1 - 0.25 % Show Material materials with Titanio of 0.1 - 0.25 % |