Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.35 % Show Material materials with Hierro of 0.35 % |
Manganeso | 4.5 - 5.5 % Show Material materials with Manganeso of 4.5 - 5.5 % |
Otro | Rest Cu, total 0.9 |
Plomo | 0.03 % Show Material materials with Plomo of 0.03 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Zinc | 0.4 % Show Material materials with Zinc of 0.4 % |