Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Antimonio | 3 - 4 % Show Material materials with Antimonio of 3 - 4 % |
Arsénico | 0.1 % Show Material materials with Arsénico of 0.1 % |
Bismuto | 0.025 % Show Material materials with Bismuto of 0.025 % |
Estaño | 0.5 % Show Material materials with Estaño of 0.5 % |
Fósforo | 0.15 - 0.3 % Show Material materials with Fósforo of 0.15 - 0.3 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Níquel | 3 - 4 % Show Material materials with Níquel of 3 - 4 % |
Otro | Rest Cu, total 0.9 |
Plomo | 18 - 22 % Show Material materials with Plomo of 18 - 22 % |
Silicona | 0.02 % Show Material materials with Silicona of 0.02 % |
Zinc | 3 - 4 % Show Material materials with Zinc of 3 - 4 % |