General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.4 - 8.9 g/cm³ Show Material materials with Densidad of 8.4 - 8.9 g/cm³ | Typical for Wrought Copper Nickel Silver Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.32 [-] Show Material materials with Coeficiente de Poisson of 0.32 [-] | Typical for Wrought Copper Nickel Silver Grade |
Módulo elástico | 23.0 °C | 120 - 140 GPa Show Material materials with Módulo elástico of 120 - 140 GPa | Typical for Wrought Copper Nickel Silver Grade |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | Typical for Wrought Copper Nickel Silver Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.9E-5 1/K | Typical for Wrought Copper Nickel Silver Grade |
Conductividad térmica | 23.0 °C | 21 - 116 W/(m·K) Show Material materials with Conductividad térmica of 21 - 116 W/(m·K) | Typical for Wrought Copper Nickel Silver Grade |
Temperatura de fusión | 875 - 1135 °C Show Material materials with Temperatura de fusión of 875 - 1135 °C | Typical for Wrought Copper Nickel Silver Grade |
Chemical properties
Property | Value |
---|---|
Antimonio | 2E-3 % Show Material materials with Antimonio of 2E-3 % |
Arsénico | 0.01 % Show Material materials with Arsénico of 0.01 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Bismuto | 2E-3 % Show Material materials with Bismuto of 2E-3 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cobre | 62 - 65 % Show Material materials with Cobre of 62 - 65 % |
Fósforo | 5E-3 % Show Material materials with Fósforo of 5E-3 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Magnesio | 0.05 % Show Material materials with Magnesio of 0.05 % |
Manganeso | 0.3 % Show Material materials with Manganeso of 0.3 % |
Níquel | 13.5 - 16.5 % Show Material materials with Níquel of 13.5 - 16.5 % |
Otro | Rest Zn, total 0.9 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % |