Chemical properties
Property | Value |
---|---|
Aluminio | 8.5 - 11 % Show Material materials with Aluminio of 8.5 - 11 % |
Cobre | 81 - 88 % Show Material materials with Cobre of 81 - 88 % |
Hierro | 3 - 5 % Show Material materials with Hierro of 3 - 5 % |
Manganeso | 0.5 - 2 % Show Material materials with Manganeso of 0.5 - 2 % |
Níquel | 0.5 - 2 % Show Material materials with Níquel of 0.5 - 2 % |