Property | Value |
---|---|
Aluminio | 9 - 12 % Show Material materials with Aluminio of 9 - 12 % |
Cobre | 80 - 87 % Show Material materials with Cobre of 80 - 87 % |
Hierro | 3 - 5 % Show Material materials with Hierro of 3 - 5 % |
Manganeso | 0.5 - 2 % Show Material materials with Manganeso of 0.5 - 2 % |
Níquel | 0.5 - 2 % Show Material materials with Níquel of 0.5 - 2 % |