Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Antimonio | 0.2 % Show Material materials with Antimonio of 0.2 % |
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % |
Cobre | 85.5 - 88.3 % Show Material materials with Cobre of 85.5 - 88.3 % |
Estaño | 10.7 - 13 % Show Material materials with Estaño of 10.7 - 13 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 1.8 % Show Material materials with Níquel of 1.8 % |
Plomo | 0.8 % Show Material materials with Plomo of 0.8 % |
Silicona | 0.01 % Show Material materials with Silicona of 0.01 % |
Zinc | 2 % Show Material materials with Zinc of 2 % |