General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.7 - 8.7 g/cm³ Show Material materials with Densidad of 7.7 - 8.7 g/cm³ | Typical for Leaded Phosphor Bronze |
Mecánica
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 380 J/(kg·K) Show Material materials with Calor específico of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Cromo | 0.01 - 0.12 % Show Material materials with Cromo of 0.01 - 0.12 % |
Estaño | 1.2 - 1.9 % Show Material materials with Estaño of 1.2 - 1.9 % |
Otro | Rest Cu+Ag |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 2.7 - 3.4 % Show Material materials with Silicona of 2.7 - 3.4 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |