General
Property | Value | Comment |
---|---|---|
Densidad | 8.47 g/cm³ Show Material materials with Densidad of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass | ||
Módulo elástico | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass | ||
Resistencia a la tracción | 448 MPa Show Material materials with Resistencia a la tracción of 448 MPa | ASTM B584 | Casting | |
483 MPa Show Material materials with Resistencia a la tracción of 483 MPa | ASTM B505 | Casting |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 335 - 390 J/(kg·K) Show Material materials with Calor específico of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Coeficiente de dilatación térmica | 1.5e-05 - 1.9e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5e-05 - 1.9e-05 1/K | Typical for Cast Copper Brass Yellow Brass |
Conductividad térmica | 116 W/(m·K) Show Material materials with Conductividad térmica of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Temperatura de fusión | 905 - 932 °C Show Material materials with Temperatura de fusión of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 0.5 - 1.5 % Show Material materials with Aluminio of 0.5 - 1.5 % | ASTM B176, ASTM B30, ASTM B505, ASTM B584 | Casting |
Cobre | 55 - 60 % Show Material materials with Cobre of 55 - 60 % | ASTM B176, ASTM B30, ASTM B505, ASTM B584 | Casting |
Estaño | 1 % Show Material materials with Estaño of 1 % | ASTM B176, ASTM B30, ASTM B505, ASTM B584 | Casting |
Hierro | 0.4 - 2 % Show Material materials with Hierro of 0.4 - 2 % | ASTM B176, ASTM B30, ASTM B505, ASTM B584 | Casting |
Manganeso | 0.1 - 1.5 % Show Material materials with Manganeso of 0.1 - 1.5 % | ASTM B176, ASTM B30, ASTM B505, ASTM B584 | Casting |
Níquel | 0.8 % Show Material materials with Níquel of 0.8 % | ASTM B30 | |
1 % Show Material materials with Níquel of 1 % | ASTM B176, ASTM B505, ASTM B584 | Casting | |
Plomo | 0.3 % Show Material materials with Plomo of 0.3 % | ASTM B30 | |
0.4 % Show Material materials with Plomo of 0.4 % | ASTM B176, ASTM B505, ASTM B584 | Casting | |
Zinc | 36 - 42 % Show Material materials with Zinc of 36 - 42 % | ASTM B176, ASTM B30, ASTM B505, ASTM B584 | Casting |