Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Bronze | ||
Módulo elástico | 96 - 120 GPa Show Material materials with Módulo elástico of 96 - 120 GPa | Typical for Cast Copper Bronze | ||
Resistencia a la tracción | 252 MPa Show Material materials with Resistencia a la tracción of 252 MPa | ASTM B505 | Casting |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 376 - 440 J/(kg·K) Show Material materials with Calor específico of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Coeficiente de dilatación térmica | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Conductividad térmica | 12 - 81 W/(m·K) Show Material materials with Conductividad térmica of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Temperatura de fusión | 760 - 1060 °C Show Material materials with Temperatura de fusión of 760 - 1060 °C | Typical for Cast Copper Bronze |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 0.005 % Show Material materials with Aluminio of 0.005 % | ASTM B30, ASTM B505 | Casting |
Antimonio | 0.2 % Show Material materials with Antimonio of 0.2 % | ASTM B30 | |
0.25 % Show Material materials with Antimonio of 0.25 % | ASTM B505 | Casting | |
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % | ASTM B30, ASTM B505 | Casting |
Cobre | 86 - 89 % Show Material materials with Cobre of 86 - 89 % | ASTM B30, ASTM B505 | Casting |
Estaño | 9 - 11 % Show Material materials with Estaño of 9 - 11 % | ASTM B505 | Casting |
9.3 - 11 % Show Material materials with Estaño of 9.3 - 11 % | ASTM B30 | ||
Fósforo | 0.25 % Show Material materials with Fósforo of 0.25 % | ASTM B30 | |
0.3 % Show Material materials with Fósforo of 0.3 % | ASTM B30 | ||
1.5 % Show Material materials with Fósforo of 1.5 % | ASTM B505 | Casting | |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % | ASTM B30 | |
0.15 % Show Material materials with Hierro of 0.15 % | ASTM B30 | ||
0.2 % Show Material materials with Hierro of 0.2 % | ASTM B505 | Casting | |
0.2 % Show Material materials with Hierro of 0.2 % | |||
Níquel | 0.8 % Show Material materials with Níquel of 0.8 % | ASTM B30 | |
1 % Show Material materials with Níquel of 1 % | ASTM B505 | Casting | |
Plomo | 1 - 2.3 % Show Material materials with Plomo of 1 - 2.3 % | ASTM B30 | |
1 - 2.5 % Show Material materials with Plomo of 1 - 2.5 % | ASTM B505 | Casting | |
Silicona | 0.005 % Show Material materials with Silicona of 0.005 % | ASTM B30, ASTM B505 | Casting |
Zinc | 0.7 % Show Material materials with Zinc of 0.7 % | ASTM B505 | Casting |
0.8 % Show Material materials with Zinc of 0.8 % | ASTM B30 |