Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Bronze |
Elongación A50 | 23.0 °C | 25 % Show Material materials with Elongación A50 of 25 % | |
Límite elástico Rp0.5 | 23.0 °C | 138 MPa Show Material materials with Límite elástico Rp0.5 of 138 MPa | |
Módulo elástico | 23.0 °C | 96 - 120 GPa Show Material materials with Módulo elástico of 96 - 120 GPa | Typical for Cast Copper Bronze |
Resistencia a la tracción | 23.0 °C | 310 MPa Show Material materials with Resistencia a la tracción of 310 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 376 - 440 J/(kg·K) Show Material materials with Calor específico of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.9E-5 1/K | Typical for Cast Copper Bronze |
Conductividad térmica | 23.0 °C | 12 - 81 W/(m·K) Show Material materials with Conductividad térmica of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Temperatura de fusión | 760 - 1060 °C Show Material materials with Temperatura de fusión of 760 - 1060 °C | Typical for Cast Copper Bronze |
Chemical properties
Property | Value |
---|---|
Aluminio | 5E-3 % Show Material materials with Aluminio of 5E-3 % |
Antimonio | 0.1 - 0.15 % Show Material materials with Antimonio of 0.1 - 0.15 % |
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % |
Cobre | 85 - 90 % Show Material materials with Cobre of 85 - 90 % |
Estaño | 4.5 - 6 % Show Material materials with Estaño of 4.5 - 6 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 0.2 - 0.25 % Show Material materials with Hierro of 0.2 - 0.25 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 4.5 - 6 % Show Material materials with Níquel of 4.5 - 6 % |
Plomo | 0.08 - 0.1 % Show Material materials with Plomo of 0.08 - 0.1 % |
Silicona | 5E-3 % Show Material materials with Silicona of 5E-3 % |
Zinc | 1 - 2.5 % Show Material materials with Zinc of 1 - 2.5 % |