Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Bronze |
Módulo elástico | 96 - 120 GPa Show Material materials with Módulo elástico of 96 - 120 GPa | Typical for Cast Copper Bronze |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 376 - 440 J/(kg·K) Show Material materials with Calor específico of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Coeficiente de dilatación térmica | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Conductividad térmica | 12 - 81 W/(m·K) Show Material materials with Conductividad térmica of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Temperatura de fusión | 760 - 1060 °C Show Material materials with Temperatura de fusión of 760 - 1060 °C | Typical for Cast Copper Bronze |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Aluminio | 10.5 - 11.5 % Show Material materials with Aluminio of 10.5 - 11.5 % | ASTM B30, ASTM B271, ASTM B505 |
Cobalto | 0.2 % Show Material materials with Cobalto of 0.2 % | ASTM B30 |
Cobre | 74.5 % Show Material materials with Cobre of 74.5 % | ASTM B30, ASTM B271, ASTM B505 |
Cromo | 0.05 % Show Material materials with Cromo of 0.05 % | ASTM B30 |
Estaño | 0.25 % Show Material materials with Estaño of 0.25 % | ASTM B30, ASTM B271, ASTM B505 |
Hierro | 4 - 5.5 % Show Material materials with Hierro of 4 - 5.5 % | ASTM B30, ASTM B271, ASTM B505 |
Magnesio | 0.05 % Show Material materials with Magnesio of 0.05 % | ASTM B30 |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % | ASTM B30, ASTM B271, ASTM B505 |
Níquel | 4.2 - 6 % Show Material materials with Níquel of 4.2 - 6 % | ASTM B30, ASTM B271, ASTM B505 |
Plomo | 0.03 % Show Material materials with Plomo of 0.03 % | ASTM B30, ASTM B271, ASTM B505 |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % | ASTM B30, ASTM B271, ASTM B505 |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % | ASTM B30, ASTM B271, ASTM B505 |