Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Nickel Grade |
Elongación A50 | 23.0 °C | 25 % Show Material materials with Elongación A50 of 25 % | |
Límite elástico Rp0.5 | 23.0 °C | 241 MPa Show Material materials with Límite elástico Rp0.5 of 241 MPa | |
Módulo elástico | 23.0 °C | 120 - 156 GPa Show Material materials with Módulo elástico of 120 - 156 GPa | Typical for Cast Copper Nickel Grade |
Resistencia a la tracción | 23.0 °C | 448 MPa Show Material materials with Resistencia a la tracción of 448 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | Typical for Cast Copper Nickel Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | Typical for Cast Copper Nickel Grade |
Conductividad térmica | 23.0 °C | 23 - 45 W/(m·K) Show Material materials with Conductividad térmica of 23 - 45 W/(m·K) | Typical for Cast Copper Nickel Grade |
Temperatura de fusión | 1100 - 1240 °C Show Material materials with Temperatura de fusión of 1100 - 1240 °C | Typical for Cast Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Aluminio | 5E-3 % Show Material materials with Aluminio of 5E-3 % |
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.15 % Show Material materials with Carbono of 0.15 % |
Cobre | 65 - 67 % Show Material materials with Cobre of 65 - 67 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 0.25 - 1.5 % Show Material materials with Hierro of 0.25 - 1.5 % |
Manganeso | 0.8 - 1.5 % Show Material materials with Manganeso of 0.8 - 1.5 % |
Níquel | 28 - 32 % Show Material materials with Níquel of 28 - 32 % |
Otro | Rest Cu |
Plomo | 0.01 - 0.03 % Show Material materials with Plomo of 0.01 - 0.03 % |
Silicona | 0.3 - 0.5 % Show Material materials with Silicona of 0.3 - 0.5 % |