Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 - 2 % Show Material materials with Aluminio of 0.5 - 2 % |
Hierro | 1 - 5.5 % Show Material materials with Hierro of 1 - 5.5 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 1 - 5.5 % Show Material materials with Níquel of 1 - 5.5 % |
Otro | Rest Cu |
Plomo | 0.25 % Show Material materials with Plomo of 0.25 % |
Silicona | 0.5 - 2 % Show Material materials with Silicona of 0.5 - 2 % |