Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 12 % Show Material materials with Elongación A50 of 12 % |
Límite elástico Rp0.5 | 23.0 °C | 276 MPa Show Material materials with Límite elástico Rp0.5 of 276 MPa |
Resistencia a la tracción | 23.0 °C | 483 MPa Show Material materials with Resistencia a la tracción of 483 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 - 2 % Show Material materials with Aluminio of 0.5 - 2 % |
Hierro | 3 - 5.5 % Show Material materials with Hierro of 3 - 5.5 % |
Manganeso | 0.2 - 0.5 % Show Material materials with Manganeso of 0.2 - 0.5 % |
Níquel | 3.5 - 5.5 % Show Material materials with Níquel of 3.5 - 5.5 % |
Otro | Rest Cu |
Plomo | 0.09 - 0.25 % Show Material materials with Plomo of 0.09 - 0.25 % |
Silicona | 0.5 - 2 % Show Material materials with Silicona of 0.5 - 2 % |
Zinc | 0.5 - 2 % Show Material materials with Zinc of 0.5 - 2 % |