Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 - 3 % Show Material materials with Aluminio of 0.5 - 3 % |
Cobre | 54 % Show Material materials with Cobre of 54 % |
Estaño | 1 % Show Material materials with Estaño of 1 % |
Hierro | 1 % Show Material materials with Hierro of 1 % |
Manganeso | 11 - 15 % Show Material materials with Manganeso of 11 - 15 % |
Níquel | 4 - 6 % Show Material materials with Níquel of 4 - 6 % |
Plomo | 2 % Show Material materials with Plomo of 2 % |
Zinc | 19 - 25 % Show Material materials with Zinc of 19 - 25 % |