Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cobre | 84.5 % Show Material materials with Cobre of 84.5 % |
Hierro | 1.2 - 1.8 % Show Material materials with Hierro of 1.2 - 1.8 % |
Manganeso | 1.2 - 1.5 % Show Material materials with Manganeso of 1.2 - 1.5 % |
Niobio | 1 % Show Material materials with Niobio of 1 % |
Níquel | 9.2 - 11 % Show Material materials with Níquel of 9.2 - 11 % |
Plomo | 0.03 % Show Material materials with Plomo of 0.03 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |