Chemical properties
Property | Value |
---|---|
Antimonio | 0.05 % Show Material materials with Antimonio of 0.05 % |
Arsénico | 0.08 % Show Material materials with Arsénico of 0.08 % |
Cobre | 78.5 - 82 % Show Material materials with Cobre of 78.5 - 82 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 0.8 % Show Material materials with Níquel of 0.8 % |
Otro | Rest Zn, total 1.0 |
Plomo | 0.6 % Show Material materials with Plomo of 0.6 % |
Silicona | 4 - 4.8 % Show Material materials with Silicona of 4 - 4.8 % |