General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 11.34 g/cm³ Show Material materials with Densidad of 11.34 g/cm³ | Typical for Pure/Low Alloyed Lead |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.4 [-] Show Material materials with Coeficiente de Poisson of 0.4 [-] | Typical for Pure/Low Alloyed Lead |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 112 - 134 J/(kg·K) Show Material materials with Calor específico of 112 - 134 J/(kg·K) | Typical for Pure/Low Alloyed Lead |
Conductividad térmica | 23.0 °C | 34 - 35 W/(m·K) Show Material materials with Conductividad térmica of 34 - 35 W/(m·K) | Typical for Pure/Low Alloyed Lead |
Temperatura de fusión | 327 °C Show Material materials with Temperatura de fusión of 327 °C | Typical for Pure/Low Alloyed Lead |
Chemical properties
Property | Value |
---|---|
Antimonio | 5E-4 % Show Material materials with Antimonio of 5E-4 % |
Arsénico | 5E-4 % Show Material materials with Arsénico of 5E-4 % |
Bismuto | 0.015 % Show Material materials with Bismuto of 0.015 % |
Cadmio | 2E-4 % Show Material materials with Cadmio of 2E-4 % |
Cobre | 1E-3 % Show Material materials with Cobre of 1E-3 % |
Estaño | 5E-4 % Show Material materials with Estaño of 5E-4 % |
Níquel | 5E-4 % Show Material materials with Níquel of 5E-4 % |
Otro | Other impurities: Total 0.015 |
Plata | 2.5E-3 % Show Material materials with Plata of 2.5E-3 % |
Plomo | 99.99 % Show Material materials with Plomo of 99.99 % |
Zinc | 2E-4 % Show Material materials with Zinc of 2E-4 % |