Chemical properties
Property | Value |
---|---|
Aluminio | 8 - 11 % Show Material materials with Aluminio of 8 - 11 % |
Cobre | 76 % Show Material materials with Cobre of 76 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 3.5 - 5.5 % Show Material materials with Hierro of 3.5 - 5.5 % |
Manganeso | 3 % Show Material materials with Manganeso of 3 % |
Níquel | 3.5 - 6.5 % Show Material materials with Níquel of 3.5 - 6.5 % |
Plomo | 0.1 % Show Material materials with Plomo of 0.1 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |