Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.5 - 1.5 % Show Material materials with Hierro of 0.5 - 1.5 % |
Manganeso | 0.6 - 1.2 % Show Material materials with Manganeso of 0.6 - 1.2 % |
Níquel | 29 - 31 % Show Material materials with Níquel of 29 - 31 % |
Otro | Rest Cu |
Plomo | 0.03 % Show Material materials with Plomo of 0.03 % |
Silicona | 0.3 - 0.7 % Show Material materials with Silicona of 0.3 - 0.7 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |