Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Nickel Grade |
Módulo elástico | 23.0 °C | 120 - 156 GPa Show Material materials with Módulo elástico of 120 - 156 GPa | Typical for Cast Copper Nickel Grade |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | Typical for Cast Copper Nickel Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | Typical for Cast Copper Nickel Grade |
Conductividad térmica | 23.0 °C | 23 - 45 W/(m·K) Show Material materials with Conductividad térmica of 23 - 45 W/(m·K) | Typical for Cast Copper Nickel Grade |
Temperatura de fusión | 1100 - 1240 °C Show Material materials with Temperatura de fusión of 1100 - 1240 °C | Typical for Cast Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Bismuto | 0.01 % Show Material materials with Bismuto of 0.01 % |
Cadmio | 0.02 % Show Material materials with Cadmio of 0.02 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.5 - 1.5 % Show Material materials with Hierro of 0.5 - 1.5 % |
Magnesio | 0.01 % Show Material materials with Magnesio of 0.01 % |
Manganeso | 0.6 - 1.2 % Show Material materials with Manganeso of 0.6 - 1.2 % |
Níquel | 29 - 31 % Show Material materials with Níquel of 29 - 31 % |
Otro | Rest Cu, total 0.15 |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % |
Selenio | 0.01 % Show Material materials with Selenio of 0.01 % |
Silicona | 0.3 - 0.7 % Show Material materials with Silicona of 0.3 - 0.7 % |
Telurio | 0.01 % Show Material materials with Telurio of 0.01 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |