Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Antimonio | 0.5 % Show Material materials with Antimonio of 0.5 % |
Arsénico | 0.15 % Show Material materials with Arsénico of 0.15 % |
Azufre | 0.08 % Show Material materials with Azufre of 0.08 % |
Estaño | 9 - 11 % Show Material materials with Estaño of 9 - 11 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Otro | Rest Cu, total 0.8 |
Plomo | 8.5 - 11 % Show Material materials with Plomo of 8.5 - 11 % |
Silicona | 0.02 % Show Material materials with Silicona of 0.02 % |
Zinc | 0.8 % Show Material materials with Zinc of 0.8 % |