Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 % Show Material materials with Aluminio of 0.5 % |
Cobre | 63 - 67 % Show Material materials with Cobre of 63 - 67 % |
Estaño | 1.5 % Show Material materials with Estaño of 1.5 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 1 % Show Material materials with Hierro of 1 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Otro | Rest Zn, total 2.0 |
Plomo | 1 - 3 % Show Material materials with Plomo of 1 - 3 % |
Silicona | 0.05 % Show Material materials with Silicona of 0.05 % |