Chemical properties
Property | Value |
---|---|
Aluminio | 4.5 - 7 % Show Material materials with Aluminio of 4.5 - 7 % |
Cobre | 64 - 68 % Show Material materials with Cobre of 64 - 68 % |
Estaño | 0.3 % Show Material materials with Estaño of 0.3 % |
Hierro | 2 - 4 % Show Material materials with Hierro of 2 - 4 % |
Manganeso | 1.5 - 4 % Show Material materials with Manganeso of 1.5 - 4 % |
Níquel | 3 % Show Material materials with Níquel of 3 % |
Otro | Rest Zn, total 0.5 |
Plomo | 0.2 % Show Material materials with Plomo of 0.2 % |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |