General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.47 g/cm³ Show Material materials with Densidad of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 335 - 390 J/(kg·K) Show Material materials with Calor específico of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Cast Copper Brass Yellow Brass |
Conductividad térmica | 23.0 °C | 116 W/(m·K) Show Material materials with Conductividad térmica of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Temperatura de fusión | 905 - 932 °C Show Material materials with Temperatura de fusión of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass |
Chemical properties
Property | Value |
---|---|
Aluminio | 5 - 6.5 % Show Material materials with Aluminio of 5 - 6.5 % |
Antimonio | 0.01 % Show Material materials with Antimonio of 0.01 % |
Arsénico | 0.02 % Show Material materials with Arsénico of 0.02 % |
Bismuto | 1E-3 % Show Material materials with Bismuto of 1E-3 % |
Cobre | 61 - 63.5 % Show Material materials with Cobre of 61 - 63.5 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | 1 - 2.5 % Show Material materials with Hierro of 1 - 2.5 % |
Manganeso | 2.5 - 3.5 % Show Material materials with Manganeso of 2.5 - 3.5 % |
Níquel | 1 - 2 % Show Material materials with Níquel of 1 - 2 % |
Otro | Rest Zn, total 1.0 |
Plomo | 0.5 % Show Material materials with Plomo of 0.5 % |
Silicona | 0.03 % Show Material materials with Silicona of 0.03 % |