Chemical properties
Property | Value |
---|---|
Aluminio | 1 - 3 % Show Material materials with Aluminio of 1 - 3 % |
Antimonio | 0.05 % Show Material materials with Antimonio of 0.05 % |
Cobre | 55 - 66 % Show Material materials with Cobre of 55 - 66 % |
Estaño | 0.3 % Show Material materials with Estaño of 0.3 % |
Hierro | 0.5 - 2.5 % Show Material materials with Hierro of 0.5 - 2.5 % |
Manganeso | 1 - 4 % Show Material materials with Manganeso of 1 - 4 % |
Níquel | 3 % Show Material materials with Níquel of 3 % |
Plomo | 0.3 % Show Material materials with Plomo of 0.3 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |