Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Manganeso | 0.7 - 1.3 % Show Material materials with Manganeso of 0.7 - 1.3 % |
Otro | Rest Cu, total 0.5 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 2.7 - 3.2 % Show Material materials with Silicona of 2.7 - 3.2 % |
Zinc | 0.4 % Show Material materials with Zinc of 0.4 % |