Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Bismuto | 0.03 % Show Material materials with Bismuto of 0.03 % |
Cadmio | 0.03 % Show Material materials with Cadmio of 0.03 % |
Fósforo | 7 - 7.6 % Show Material materials with Fósforo of 7 - 7.6 % |
Níquel | 0.05 - 0.15 % Show Material materials with Níquel of 0.05 - 0.15 % |
Otro | Rest Cu, Zn+Cd < 0.05, Alle Total 0.25 |
Plata | 5.5 - 6.5 % Show Material materials with Plata of 5.5 - 6.5 % |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % |