Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Antimonio | 1.8 - 2.2 % Show Material materials with Antimonio of 1.8 - 2.2 % |
Bismuto | 0.03 % Show Material materials with Bismuto of 0.03 % |
Cadmio | 0.03 % Show Material materials with Cadmio of 0.03 % |
Fósforo | 5.6 - 6.4 % Show Material materials with Fósforo of 5.6 - 6.4 % |
Otro | Rest Cu, Zn+Cd < 0.05, Alle Total 0.25 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % |