Chemical properties
Property | Value |
---|---|
Aluminio | 1E-3 % Show Material materials with Aluminio of 1E-3 % |
Bismuto | 0.03 % Show Material materials with Bismuto of 0.03 % |
Cadmio | 0.03 % Show Material materials with Cadmio of 0.03 % |
Cobre | 35 - 37 % Show Material materials with Cobre of 35 - 37 % |
Estaño | 2 - 3 % Show Material materials with Estaño of 2 - 3 % |
Fósforo | 8E-3 % Show Material materials with Fósforo of 8E-3 % |
Otro | total 0.15 |
Plata | 33 - 35 % Show Material materials with Plata of 33 - 35 % |
Plomo | 0.03 % Show Material materials with Plomo of 0.03 % |
Silicona | 0.05 % Show Material materials with Silicona of 0.05 % |
Zinc | 25.5 - 29.5 % Show Material materials with Zinc of 25.5 - 29.5 % |