Chemical properties
Property | Value |
---|---|
Aluminio | 5.5 - 6.5 % Show Material materials with Aluminio of 5.5 - 6.5 % |
Cobre | 72 - 78 % Show Material materials with Cobre of 72 - 78 % |
Hierro | 1.5 - 2.5 % Show Material materials with Hierro of 1.5 - 2.5 % |
Manganeso | 9 - 14 % Show Material materials with Manganeso of 9 - 14 % |
Níquel | 1.5 - 2.5 % Show Material materials with Níquel of 1.5 - 2.5 % |
Otro | Alle Total 0.5 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |