Chemical properties
Property | Value |
---|---|
Aluminio | 9 - 10 % Show Material materials with Aluminio of 9 - 10 % |
Hierro | 0.5 - 1.5 % Show Material materials with Hierro of 0.5 - 1.5 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Otro | Rest Cu, total 0.2 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |