Chemical properties
Property | Value |
---|---|
Aluminio | 8.5 - 9.5 % Show Material materials with Aluminio of 8.5 - 9.5 % |
Hierro | 2.5 - 4 % Show Material materials with Hierro of 2.5 - 4 % |
Manganeso | 1 - 2 % Show Material materials with Manganeso of 1 - 2 % |
Níquel | 3.5 - 5.5 % Show Material materials with Níquel of 3.5 - 5.5 % |
Otro | Rest Cu, total 0.2 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |