Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Cobre | 46 - 50 % Show Material materials with Cobre of 46 - 50 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.25 % Show Material materials with Hierro of 0.25 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 8 - 11 % Show Material materials with Níquel of 8 - 11 % |
Otro | Rest Zn, total 0.2 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % |