Chemical properties
Property | Value |
---|---|
Aluminio | 1E-3 % Show Material materials with Aluminio of 1E-3 % |
Antimonio | 0.01 % Show Material materials with Antimonio of 0.01 % |
Arsénico | 1E-3 % Show Material materials with Arsénico of 1E-3 % |
Bismuto | 0.01 % Show Material materials with Bismuto of 0.01 % |
Cadmio | 0.03 % Show Material materials with Cadmio of 0.03 % |
Cobre | 58.5 - 61.5 % Show Material materials with Cobre of 58.5 - 61.5 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.25 % Show Material materials with Hierro of 0.25 % |
Manganeso | 0.05 - 0.25 % Show Material materials with Manganeso of 0.05 - 0.25 % |
Otro | Rest Zn, total 0.2. excluded Fe |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % |