Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Cobre | 56 - 60 % Show Material materials with Cobre of 56 - 60 % |
Estaño | 0.8 - 1.1 % Show Material materials with Estaño of 0.8 - 1.1 % |
Hierro | 0.25 - 1.2 % Show Material materials with Hierro of 0.25 - 1.2 % |
Manganeso | 0.01 - 0.5 % Show Material materials with Manganeso of 0.01 - 0.5 % |
Otro | Rest Zn, total 0.2 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.04 - 0.15 % Show Material materials with Silicona of 0.04 - 0.15 % |