Chemical properties
Property | Value |
---|---|
Aluminio | 1E-3 % Show Material materials with Aluminio of 1E-3 % |
Bismuto | 0.03 % Show Material materials with Bismuto of 0.03 % |
Cadmio | 0.03 % Show Material materials with Cadmio of 0.03 % |
Cobre | 43 - 45 % Show Material materials with Cobre of 43 - 45 % |
Fósforo | 8E-3 % Show Material materials with Fósforo of 8E-3 % |
Otro | total 0.15 |
Plata | 19 - 21 % Show Material materials with Plata of 19 - 21 % |
Plomo | 0.03 % Show Material materials with Plomo of 0.03 % |
Silicona | 0.05 - 0.25 % Show Material materials with Silicona of 0.05 - 0.25 % |