Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Antimonio | 0.02 % Show Material materials with Antimonio of 0.02 % |
Arsénico | 0.02 % Show Material materials with Arsénico of 0.02 % |
Bismuto | 5E-3 % Show Material materials with Bismuto of 5E-3 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Estaño | 0.05 % Show Material materials with Estaño of 0.05 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Magnesio | 0.05 % Show Material materials with Magnesio of 0.05 % |
Manganeso | 29 - 31 % Show Material materials with Manganeso of 29 - 31 % |
Otro | Rest Cu, each 0.05, total 0.3 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Selenio | 5E-3 % Show Material materials with Selenio of 5E-3 % |
Silicona | 0.05 % Show Material materials with Silicona of 0.05 % |
Telurio | 5E-3 % Show Material materials with Telurio of 5E-3 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |