Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Estaño | 0.05 % Show Material materials with Estaño of 0.05 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 48.5 - 51.5 % Show Material materials with Níquel of 48.5 - 51.5 % |
Otro | Rest Cu, each 0.05, total 0.3 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.05 % Show Material materials with Silicona of 0.05 % |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % |