Property | Value |
---|---|
Aluminio | 0.1 % Show Material materials with Aluminio of 0.1 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.7 % Show Material materials with Hierro of 0.7 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Otro | Rest Cu, each 0.1, total 0.5 |
Plomo | 0.2 % Show Material materials with Plomo of 0.2 % |
Silicona | 28 - 32 % Show Material materials with Silicona of 28 - 32 % |