Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Bismuto | 5E-3 % Show Material materials with Bismuto of 5E-3 % |
Circonio | 49 - 53 % Show Material materials with Circonio of 49 - 53 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Fósforo | 0.1 % Show Material materials with Fósforo of 0.1 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Niobio | 2 % Show Material materials with Niobio of 2 % |
Otro | Rest Cu, each 0.1, total 0.5 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.05 % Show Material materials with Silicona of 0.05 % |
Telurio | 5E-3 % Show Material materials with Telurio of 5E-3 % |