Chemical properties
Property | Value |
---|---|
Aluminio | 0.1 % Show Material materials with Aluminio of 0.1 % |
Bismuto | 5E-3 % Show Material materials with Bismuto of 5E-3 % |
Estaño | 0.05 % Show Material materials with Estaño of 0.05 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Otro | Rest Cu, each 0.05, total 0.3 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.05 % Show Material materials with Silicona of 0.05 % |
Telurio | 5E-3 % Show Material materials with Telurio of 5E-3 % |
Titanio | 28.5 - 31.5 % Show Material materials with Titanio of 28.5 - 31.5 % |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % |