Chemical properties
Property | Value |
---|---|
Aluminio | 2E-3 % Show Material materials with Aluminio of 2E-3 % |
Bismuto | 5E-4 % Show Material materials with Bismuto of 5E-4 % |
Cobre | 99.9 % Show Material materials with Cobre of 99.9 % |
Estaño | 2E-3 % Show Material materials with Estaño of 2E-3 % |
Fósforo | 1E-3 % Show Material materials with Fósforo of 1E-3 % |
Hierro | 2E-3 % Show Material materials with Hierro of 2E-3 % |
Níquel | 2E-3 % Show Material materials with Níquel of 2E-3 % |
Otro | Cu: including Ag to max. 0.015% and O to 0.06%, each 0.002 |
Plomo | 5E-3 % Show Material materials with Plomo of 5E-3 % |
Zinc | 2E-3 % Show Material materials with Zinc of 2E-3 % |