Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Arsénico | 5E-3 % Show Material materials with Arsénico of 5E-3 % |
Cobre | 99.5 % Show Material materials with Cobre of 99.5 % |
Estaño | 0.06 % Show Material materials with Estaño of 0.06 % |
Fósforo | 0.06 % Show Material materials with Fósforo of 0.06 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Níquel | 0.02 % Show Material materials with Níquel of 0.02 % |
Otro | Cu: including Ag to max. 0.015% and O to 0.06%, each 0.002 |
Plomo | 0.1 % Show Material materials with Plomo of 0.1 % |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % |