Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 98 % Show Material materials with Cobre of 98 % |
Estaño | 0.25 % Show Material materials with Estaño of 0.25 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Níquel | 0.1 % Show Material materials with Níquel of 0.1 % |
Otro | Cu: including Ag to max. 0.015% and O to 0.06% |
Plomo | 0.5 % Show Material materials with Plomo of 0.5 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |