Chemical properties
Property | Value |
---|---|
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cobalto | 0.1 % Show Material materials with Cobalto of 0.1 % |
Estaño | 0.5 % Show Material materials with Estaño of 0.5 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 1.5 - 2.5 % Show Material materials with Hierro of 1.5 - 2.5 % |
Manganeso | 1.5 - 2.5 % Show Material materials with Manganeso of 1.5 - 2.5 % |
Níquel | 29 - 32 % Show Material materials with Níquel of 29 - 32 % |
Otro | Rest Cu, total 0.2 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |