Chemical properties
Property | Value |
---|---|
Aluminio | 0.4 % Show Material materials with Aluminio of 0.4 % |
Cobre | 57 % Show Material materials with Cobre of 57 % |
Estaño | 0.6 % Show Material materials with Estaño of 0.6 % |
Hierro | 0.6 % Show Material materials with Hierro of 0.6 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Otro | Rest Zn, total 0.4, Al+Fe+Ni+Sn+Others total< 1.7%, in case of CuZn38Pb4 (CW609N) Pb < 4.2% |
Plomo | 3.5 % Show Material materials with Plomo of 3.5 % |