Chemical properties
Property | Value |
---|---|
Arsénico | 0.02 - 0.06 % Show Material materials with Arsénico of 0.02 - 0.06 % |
Cobre | 70 - 72.5 % Show Material materials with Cobre of 70 - 72.5 % |
Estaño | 0.9 - 1.3 % Show Material materials with Estaño of 0.9 - 1.3 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.07 % Show Material materials with Hierro of 0.07 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 0.1 % Show Material materials with Níquel of 0.1 % |
Otro | Rest Zn, total 0.3 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |